Interesting facts about Tin in steel

SnMelting point 232 °CTin

Steel parasite as it concentrates like Cu under the scale film, penetrates along the grain boundaries and causes cracking and solder brittleness. Sn tends towards pronounced segregation and restricts the γ-phase.